Категория | Perfluoropolymer |
Производитель | Solvay Specialty Polymers |
Торговая марка | Hyflon® MFA® |
Порт | Китай Шанхайский порт |
Торговые условия | FOB, CFR, CIF |
Платежное средство | L/C, T/T, Western Union |
QQkr5S_HyflonMFAP6022.pdf | |
Контактная информация | Служба поддержки клиентов Вичат |
|
Главная Информация | |
---|---|
Характеристики |
|
Используется |
|
Внешний вид |
|
Формы |
|
Метод обработки |
|
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|---|---|---|
Удельный вес | 2.15 | g/cm³ | ASTM D792 |
Массовый расход расплава (MFR) (372°C/5.0 kg) | 2.0 - 5.0 | g/10 min | ASTM D1238 |
Средний размер частиц 1 | 300 | µm | Internal method |
Тепловой | Номинальное значение | Единица измерения | Метод испытания |
---|---|---|---|
Температура плавления | 285 | °C | ASTM D4591 |
Дополнительная информация |
---|
ProcessingHyflon MFA® P6022 can be processed using normal rotomolding/rotolining techniques. In the case of rotomolding Hyflon® MFA P6022 is initially introduced into a mold. This is then heated in an oven and maintained under rotation to achieve the desired mould shape. Finally mold extraction and cooling are carried out toobtain the final item. In rotolining the resin is directly fed inside the part to be lined, properly prepared and primered. As in the case of rotomolding, the part is then heated, maintained under rotation and finally cooled to obtain the lined article. Hyflon® MFA P6022 can be used neat and without any further formulation. Substrate preparation, MFA load, rotation parameters, oven temperature and time must all be well controlled to achieve defect free items.Storage and Handling Hyflon® melt processable fluropolymer resins can be stored without shelf life issues when kept in a clean and dry area at ambient temperatures. Opened containers should be tightly resealed to prevent any contamination. Safety and Toxicology Before using Hyflon® melt processable fluropolymer resins consult the product Material Safety Data Sheet and follow all label directions and handling precautions. As with all fluoropolymer materials, handling and processing should only be carried out in well ventilated areas. Vapor extractor units should be installed above processing equipment. Fumes must not be inhaled and eye and skin contact ought to be avoided. In case of skin contact wash with soap and water. In case of eye contact flush with water immediately and seek medical help. Do not smoke in areas contaminated with powder, vapor or fumes. See Material Safety Data Sheet for detailed advice on waste disposal methods. Packaging Hyflon® MFA P6022 is packaged in 10kg non returnable drums. Each drum has two bags liner made of polyethylene resin. |
Примечание | |
---|---|
1 . | Laser Diffraction |
Тип материала | Категория | Производитель |
---|---|---|
Hyflon® MFA® D 5510 F | Perfluoropolymer | Solvay Specialty Polymers |
Hyflon® MFA® XPH 5510_1N | Perfluoropolymer | Solvay Specialty Polymers |
Hyflon® MFA® P6310 | Perfluoropolymer | Solvay Specialty Polymers |
Hyflon® MFA® P6010 | Perfluoropolymer | Solvay Specialty Polymers |
Hyflon® AD 40H | Perfluoropolymer | Solvay Specialty Polymers |
Hyflon® AD 60 | Perfluoropolymer | Solvay Specialty Polymers |
Телефон | +086 13424755533 |