Andur 9-3 APLF/Curene® 442
Описание материалов:
Andur 9-3 APLF is a polyester based liquid, toluene diisocyanate terminated prepolymer containing 0.1% or less free TDI monomer. An elastomer with a hardness of 92 to 94 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442, other diamines or through the use of plasticizers.
| Твердость | Номинальное значение | | Метод испытания |
|---|
| Твердость дюрометра (Shore A) | 93 | | ASTM D2240 |
| Эластомеры | Номинальное значение | Единица измерения | Метод испытания |
|---|
| Tensile Stress | | | ASTM D412 |
| 100% strain | 9.83 | MPa | ASTM D412 |
| 300% strain | 17.6 | MPa | ASTM D412 |
| Прочность на растяжение (Yield) | 61.4 | MPa | ASTM D412 |
| Удлинение при растяжении (Break) | 530 | % | ASTM D412 |
| Термокомплект | Номинальное значение | Единица измерения | |
|---|
| Срок службы горшка | 5.0 - 6.0 | min | |
| Время демолд (100°C) | 20 - 30 | min | |
| Время доставки (100°C) | 16 | hr | |
| Дополнительная информация |
|---|
| Durometer Hardness, ASTM D2240, Shore A: 92 to 94Die C Tear, ASTM D1004: 500 pliAverage Split Tear, ASTM D1938: 315 pliStoichiometry Curative Level: 95%Mix Temperature:
Andur 9-3 APLF: 150-170°F
Curene 442: 230-240°F |