Описание материалов:
Andur 5-DPLM is a polyester based, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 50 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by curing Andur 5-DPLM with poyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.24 | g/cm³ | ASTM D792 |
Термокомплект | Номинальное значение | Единица измерения | Метод испытания |
---|
Терморегулирующая вязкость | | | ASTM D2393 |
21°C | 105000 | cP | ASTM D2393 |
70°C | 2000 | cP | ASTM D2393 |
100°C | 450 | cP | ASTM D2393 |
Дополнительная информация |
---|
NCO: 5.5 to 5.9%Specific Gravity, ASTM D792, 70°F: 1.24 g/mlSpecific Gravity, ASTM D792, 212°F: 1.2 g/ml |