Описание материалов:
XJ-VDE CHLORINATED POLYETHYLENE (CPE) COMPOND FOR VDE STANDARD CABLE'S INSULATION JACKETS
PRODUCT FEATURES:
Various grades of CPE compound for cable & wire's insulation jackets can be designed & produced according to the European standard. This compound is mainly produced with CPE/EPDM mix, it has good processing ability, excellent insulating property and air-bomb ageing resistance, at the same time, it can reduce the cost greatly compared to its solely compound EPDM.
MAIN APPLICATION:
This product can be used to manufacture kinds of insulating rubber cable & wire which is to meet different European standards in the application of cable core such as H05RR-F(YZ), H05RN-F(YZW), H07RN-F(YCW), etc.
| Главная Информация | |
|---|
| Характеристики | |
| Используется | - Кабельный кожух
- Кожух провода
|
| Рейтинг агентства | |
| Эластомеры | Номинальное значение | Единица измерения | |
|---|
| Tensile Stress | | | |
| Break 1 | > 4.20 | MPa | |
| Break 2 | > 5.00 | MPa | |
| Удлинение при растяжении 3(Break) | > 250 | % | |
| Старение | Номинальное значение | Единица измерения | |
|---|
| Изменение напряжения при растяжении | | | |
| 80°C, 168 hr, in Air oven | -25 to 25 | % | |
| 127°C, 40 hr, in Air bomb, 0.55 MPa | -30 to 30 | % | |
| Изменение натяжения при разрыве | | | |
| 80°C, 168 hr, in Air oven | -25 to 25 | % | |
| 127°C, 40 hr, in Air bomb, 0.55 MPa | -30 to 30 | % | |
| Воспламеняемость | Номинальное значение | Единица измерения | |
|---|
| Индекс кислорода | > 20 | % | |
| Примечание |
|---|
| 1 . | After Oven ageing test |
| 2 . | Before ageing test |
| 3 . | After Oven ageing test |