Описание материалов:
Eastman Neostar™ Elastomer FN005 is a tough, clear, durable, general purpose grade copolyester ether. It was designed for use in the profile and automotive markets, but is also used in packaging and tubing applications where toughness and flex-crack resistance are required. Eastman Neostar™ Elastomer FN005 can be used in injection molding and cast film or tubing extrusion applications or in any application that demands strength, durability, and puncture resistance in harsh environments. This copolyester combines toughness, clarity, and flexibility without the addition of plasticizers. Eastman Neostar™ Elastomer FN005 is considered environmentally preferred because of its non-halogenated material composition. The target inherent viscosity of this product is 1.05.
This product has been CRADLE TO CRADLE CERTIFIED Silver.
The CRADLE TO CRADLE CERTIFIED Mark is a registered certification mark used under license through McDonough Braungart Design Chemistry (MBDC). MBDC is a global sustainability consulting and product certification firm. The CRADLE TO CRADLE® framework moves beyond the traditional goal of reducing the negative impacts of commerce ('eco-efficiency'), to a new paradigm of increasing its positive impacts ('eco-effectiveness'). At its core, Cradle to Cradle design perceives the safe and productive processes of nature's 'biological metabolism' as a model for developing a 'technical metabolism' flow of industrial materials. Product components can be designed for continuous recovery and reutilization as biological and technical nutrients within these metabolisms. For more information about MBDC and to obtain printable certificates for Eastman Copolyesters, visit www.mbdc.com. Choose Eastman Chemical Company under Company Name in C2C Certified products to display a list of our products.
Главная Информация | |
---|
Характеристики | - Прочный
- Общее назначение
- Хорошая химическая стойкость
- Хорошее сопротивление трещине
- Хорошая стабильность размеров
- Хорошая гибкость
- Хорошая прочность
- Хорошая прочность
- Без галогенов
- Высокая четкость
- Высокая термостойкость
- Стойкий к проколу
|
Используется | - Автомобильные Приложения
- Общее назначение
- Упаковка
- Профили
- Трубка
|
Внешний вид | |
Формы | |
Метод обработки | - Литая пленка
- Литье под давлением
- Экструзионный профиль
|
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.13 | g/cm³ | ASTM D792 |
Массовый расход расплава (MFR) (230°C/2.16 kg) | 20 | g/10 min | ASTM D1238 |
Поглощение воды (23°C, 24 hr) | 0.35 | % | ASTM D570 |
Внутренняя вязкость 1(23°C) | 1.1 | | Internal Method |
Тепловой | Номинальное значение | Единица измерения | Метод испытания |
---|
Тепло плавления (23°C) | 27.0 | kJ/kg | ASTM E793 |
Дополнительная информация | Номинальное значение | Единица измерения | Метод испытания |
---|
Tear Strength (23°C) | 370 | N | ASTM D1004 |
Твердость | Номинальное значение | Единица измерения | Метод испытания |
---|
Твердость дюрометра | | | ASTM D2240 |
Shore A, 23°C | 95 | | |
Shore D, 23°C | 55 | | |
Механические | Номинальное значение | Единица измерения | Метод испытания |
---|
Модуль растяжения (23°C) | 170 | MPa | ASTM D638 |
Прочность на растяжение | | | ASTM D638 |
Yield, 23°C, 3.00 mm, Injection Molded 2 | 14.0 | MPa | |
Break, 23°C, 2.00 mm 3 | 20.0 | MPa | |
Удлинение при растяжении | | | ASTM D638 |
Yield, 23°C | 30 | % | |
Break, 23°C | 300 | % | |
Флекторный модуль (23°C) | 150 | MPa | ASTM D790 |
Коэффициент трения 4 | > 1.0 | | ASTM D1894 |
Пленки | Номинальное значение | Единица измерения | Метод испытания |
---|
Толщина пленки протестирована | 130 | µm | |
Сектантный модуль | | | ASTM D882 |
Tangent, MD
: 130 µm | 185 | MPa | |
Tangent, TD
: 130 µm | 179 | MPa | |
Прочность на растяжение | | | ASTM D882 |
MD
: Yield, 130 µm | 13.7 | MPa | |
TD
: Yield, 130 µm | 13.5 | MPa | |
MD
: Break, 130 µm | 23.7 | MPa | |
TD
: Break, 130 µm | 22.6 | MPa | |
Удлинение при растяжении | | | ASTM D882 |
MD
: Yield, 130 µm | 26 | % | |
TD
: Yield, 130 µm | 26 | % | |
MD
: Break, 130 µm | 550 | % | |
TD
: Break, 130 µm | 550 | % | |
Проницаемость кислорода (30°C, 130 µm) | 841 | cm³/m²/24 hr | ASTM D1434 |
Передача водяного пара 5 | 130 | g/m²/24 hr | ASTM F372 |
Эластомеры | Номинальное значение | Единица измерения | Метод испытания |
---|
Модуль Clash-Berg | | | ASTM D1043 |
-70°C | 930 | MPa | |
-28°C | 240 | MPa | |
Воздействие | Номинальное значение | Единица измерения | Метод испытания |
---|
Зубчатый изод Impact (-40°C) | 50 | J/m | ASTM D256 |
Тепловой | Номинальное значение | Единица измерения | Метод испытания |
---|
Температура ломкости | < -75.0 | °C | ASTM D746 |
Температура перехода стекла | -3.00 | °C | DSC |
Викат Температура размягчения | 170 | °C | ASTM D1525 6 |
Пиковая температура плавления | 207 | °C | ASTM D3418 |
Пиковая температура кристаллизации (DSC) | 140 | °C | DSC |
CLTE-
Поток (23°C) | 1.5E-4 | cm/cm/°C | ASTM D696 |
Удельный нагрев | | | DSC |
25°C 7 | 1600 | J/kg/°C | |
100°C 8 | 1800 | J/kg/°C | |
150°C 9 | 2000 | J/kg/°C | |
175°C 10 | 2300 | J/kg/°C | |
200°C 11 | 3100 | J/kg/°C | |
225°C 12 | 2300 | J/kg/°C | |
Теплопроводность (23°C) | 0.19 | W/m/K | ASTM C177 |
Примечание |
---|
1 . | EMN-A-AC-G-V-1 |
2 . | Type I, 500 mm/min |
3 . | Type IV, 500 mm/min |
4 . | 0.13 mm |
5 . | 0.13 mm |
6 . | Loading 1 (10 N) |
7 . | Solid |
8 . | Solid |
9 . | Solid |
10 . | Solid |
11 . | Transition, apparent specific heat, including the effects of the heat of fusion. |
12 . | Melt |
Тип материала |
Категория |
Производитель |
Neostar™ FN007 |
Copolyester Elastomer (Ether) |
Eastman Chemical Company
|
Neostar™ FN005 |
Copolyester Elastomer (Ether) |
Eastman Chemical Company
|
Neostar™ FN006 |
Copolyester Elastomer (Ether) |
Eastman Chemical Company
|