Описание материалов:
Eraclene FB 506 is a high density polyethylene resin (HDPE), hexene copolymer, with antioxidants, suitable for blown film extrusion.
Its broad molecular weight distribution and density successfully combine excellent performance at high extrusion rates with high films strength and sealability.
Main Application
Eraclene FB 506 can be processed either in blend and in coextrusion. It is possible to use it pure for high rigidity grocery sacks and shopping bags. Usage in blend and/or in coextrusion with LDPE and LLDPE is also recommended for high strength thermo-shrinkable film, as well as for hygienic packaging. The excellent balance between drawability and bubble stability makes Eraclene FB 506 the optimum choice for manufacturing of high quality thin films characterized by outstanding mechanical properties.
Главная Информация | |
---|
Добавка | |
Характеристики | - Антиоксидант
- Сополимер
- Приемлемый пищевой контакт
- Хорошее тепловое уплотнение
- Гексен-комномер
- Высокая плотность
- Высокая прочность
- Средний Молекулярный вес.
|
Используется | - Сумки
- Смешивание
- Пленка
- Упаковка
- Термоусадочная пленка
|
Рейтинг агентства | - ЕС пищевой контакт, неуказанный рейтинг
|
Формы | |
Метод обработки | - Выдувная пленка
- Коэкструзия
|
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Плотность | 0.939 | g/cm³ | ISO 1183 |
Массовый расход расплава (MFR) | | | ISO 1133 |
190°C/21.6 kg | 20 | g/10 min | |
190°C/5.0 kg | 0.80 | g/10 min | |
Пленки | Номинальное значение | Единица измерения | Метод испытания |
---|
Толщина пленки протестирована | 25 | µm | |
Толщина пленки-рекомендовано/доступно | 10 to 50µm | | |
Модуль растяжения | | | ISO 527-3 |
1% Secant, MD
: 25 µm, Blown Film | 400 | MPa | |
1% Secant, TD
: 25 µm, Blown Film | 500 | MPa | |
Tensile Stress | | | ISO 527-3 |
MD
: Break, 25 µm, Blown Film | 50.0 | MPa | |
TD
: Break, 25 µm, Blown Film | 50.0 | MPa | |
Удлинение при растяжении | | | ISO 527-3 |
MD
: Break, 25 µm, Blown Film | 500 | % | |
TD
: Break, 25 µm, Blown Film | 750 | % | |
Ударное падение Dart 1(25 µm, Blown Film) | 120 | g | ISO 7765-1 |
Elmendorf Tear Strength 2 | | | ISO 6383-2 |
MD
: 25.0 µm | 15.0 | kN/m | |
TD
: 25.0 µm | 180.0 | kN/m | |
Тепловой | Номинальное значение | Единица измерения | Метод испытания |
---|
Температура ломкости | < -60.0 | °C | ASTM D746 |
Викат Температура размягчения | 119 | °C | ISO 306/A |
Температура плавления | 129 | °C | Internal Method |
Экструзия | Номинальное значение | Единица измерения | |
---|
Температура расплава | 190 to 210 | °C | |
Примечание |
---|
1 . | F50 |
2 . | Blown Film |