Описание материалов:
Eastman Tritan MP200 is an amorphous copolyester that combines excellent clarity and toughness with outstanding heat and chemical resistance. Film and sheet manufactured from this new-generation copolyester can be thermoformed with a wide processing window that allows for product designs that reflect intricate detail. Eastman Tritan MP200 copolyester is suitable for use with most forms of sterilization including radiation and ethylene oxide. It is NOT suitable for autoclave/steam sterilization. Eastman Tritan MP200 copolyester has been formulated for use in medical film, sheet, and packaging applications.
Главная Информация | |
---|
Характеристики | - Радиационная дезинфекция
- Подсветка
- Дезинфекция скороварки
- Дезинфекция оксида этилена
- Хорошая химическая стойкость
- Теплостойкость, высокая
- Высокое разрешение
- Хорошая прочность
- Аморфный
- Паровая дезинфекция
|
Используется | - Упаковка
- Пленка
- Лист
- Медицинская упаковка
|
Рейтинг агентства | |
Метод обработки | - Экструзионная пленка
- Экструзия
- Экструзионный лист
- Термоформовка
|
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Плотность | 1.19 | g/cm³ | ASTM D1505 |
Поглощение воды (24 hr) | 0.50 | % | ASTM D570 |
Механические | Номинальное значение | Единица измерения | Метод испытания |
---|
Износостойкость (23 °C) 1 | 20% Haze | | ASTM D1044 |
Пленки | Номинальное значение | Единица измерения | Метод испытания |
---|
Проницаемость углекислого газа (23 °C, 254,0 мкм) | 210 | cm³·mm/m²/atm/24 hr | ASTM D1434 |
Рпт сопротивление разрыву | | | ASTM D2582 |
MD
: 23°C, 254.0 µm | 40 | N | ASTM D2582 |
TD
: 23°C, 254.0 µm | 40 | N | ASTM D2582 |
Сопротивление размножению разрыва | | | ASTM D1938 |
MD, Split Tear Method
: 23°C, 254.0 µm | 310 | gf | ASTM D1938 |
TD, Split Tear Method
: 23°C, 254.0 µm | 200 | gf | ASTM D1938 |
Оптический | Номинальное значение | Единица измерения | Метод испытания |
---|
UV Transmittance 2 | 89 | % | |
Дополнительная информация | Номинальное значение | Единица измерения | Метод испытания |
---|
Энергия поверхности | | | ASTM D5946 |
Dispersive
: 23°C | 39 | dyne/cm | ASTM D5946 |
Polar
: 23°C | 8 | dyne/cm | ASTM D5946 |
Total
: 23°C | 47 | dyne/cm | ASTM D5946 |
Пленки | Номинальное значение | Единица измерения | Метод испытания |
---|
Толщина пленки протестирована | 250 | µm | ASTM D374 |
Эластичный модуль-
MD (250 µm) | 1500 | MPa | ASTM D882 |
Эластичный модуль-
TD (250 µm) | 1400 | MPa | ASTM D882 |
Прочность на растяжение | | | ASTM D882 |
MD
: Yield, 250 µm | 43.0 | MPa | ASTM D882 |
TD
: Yield, 250 µm | 41.0 | MPa | ASTM D882 |
MD
: Break, 250 µm | 57.0 | MPa | ASTM D882 |
TD
: Break, 250 µm | 42.0 | MPa | ASTM D882 |
Удлинение при растяжении | | | ASTM D882 |
MD
: Yield, 250 µm | 8.0 | % | ASTM D882 |
TD
: Yield, 250 µm | 8.0 | % | ASTM D882 |
MD
: Break, 250 µm | 110 | % | ASTM D882 |
TD
: Break, 250 µm | 120 | % | ASTM D882 |
Ударное падение Dart 3 | | | ASTM D1709A |
-30°C, 250 µm | 850 | g | ASTM D1709A |
-18°C, 250 µm | 830 | g | ASTM D1709A |
23°C, 250 µm | 830 | g | ASTM D1709A |
Elmendorf Tear Strength | | | ASTM D1922 |
MD
: 250 µm | 380 | g | ASTM D1922 |
TD
: 250 µm | 430 | g | ASTM D1922 |
Сопротивление разрыву брюк 4 | | | ISO 6383-1 |
MD
: 250 µm | 10.0 | N/mm | ISO 6383-1 |
TD
: 250 µm | 9.00 | N/mm | ISO 6383-1 |
Проницаемость кислорода (23°C, 250 µm) | 44 | cm³·mm/m²/atm/24 hr | ASTM D3985 |
Скорость передачи водяного пара | | | ASTM F1249 |
23°C, 100% RH, 250 µm | 4.0 | g/m²/24 hr | ASTM F1249 |
38°C, 100% RH, 250 µm | 10 | g/m²/24 hr | ASTM F1249 |
Воздействие | Номинальное значение | Единица измерения | Метод испытания |
---|
Ударное устройство для дротиков (23°C, 0.254 mm, Total Energy) | 4.50 | J | ASTM D3763 |
Тепловой | Номинальное значение | Единица измерения | Метод испытания |
---|
Температура перехода стекла | 119 | °C | DSC |
CLTE-
Поток (23°C) | 8.0E-5 | cm/cm/°C | ASTM D696 |
Удельный нагрев | | | DSC |
60°C | 1700 | J/kg/°C | DSC |
100°C | 1900 | J/kg/°C | DSC |
150°C | 2300 | J/kg/°C | DSC |
200°C | 2400 | J/kg/°C | DSC |
250°C | 2600 | J/kg/°C | DSC |
Оптический | Номинальное значение | Единица измерения | Метод испытания |
---|
Блеск (60°, 254 µm) | 158 | | ASTM D2457 |
Индекс преломления | 1.540 | | ASTM D542 |
Коэффициент пропускания (Total, 254 µm) | 93.0 | % | ASTM D1003 |
Haze (254 µm) | 0.80 | % | ASTM D1003 |
Yellowness Index (0.254 mm) | 0.50 | YI | ASTM D1925 |
Примечание |
---|
1 . | 25 cycles |
2 . | UV/Vis Spectro, 380 nm |
3 . | 12.7 mm dia. head, 127 mm dia. clamp, 600 mm drop |
4 . | 200 mm/min |