Описание материалов:
Sanitary gasket made from Fluoraz® 784 work well in SIP and CIP applications where a low durometer elastomer compound is needed. While EPDMs and FKMs can provide a seal for extended periods, change in physical properties can have adverse effects beyond simple volume swell. A decrease in hardness or drop in modulus signals a reduction in compressive strength. If a sanitary gasket is retorqued ot the installation specification, th gasket will be compressed at a greater level than desired, resulting in increased intrusion into the process stream. An increase in hardness/modulus and a drop in elongation means embrittlement. The seal will be undertorqued, resulting in either leaks or cracking.
Fluoraz 784 is formulated for use in sanitary gaskets and other applications where low sealing force is required, such as sealing sight glasses or as a seal between nonmetal parts. Fluoraz 784 is FDA and USP Class VI compliant, making it a versatile compound for both pharmaceautical and other hygienic fluid handling applications. Fluoraz 784 metal and TOC extractables are an order of magnitude lower than premium competitive FKM formulations, ensuring little or not contamination into the process stream. Fluoraz 784 cna be used as a sanitary gasket in standard applications as long as the torque used to install the gasket is minimal (hand tight).
Fluoraz 784 is alos available in O-rings and custom shapes where a low durometer hardness is desired.
Главная Информация | |
---|
Характеристики | - Хорошая химическая стойкость
- Хорошее тепловое уплотнение
- Низкий уровень извлечения
- Низкая Твердость
- Устойчивость к пару
|
Используется | - Прокладки
- Фармацевтика
- Уплотнения
|
Рейтинг агентства | - FDA неуказанный рейтинг
- USP 87
- USP класс VI
|
Внешний вид | |
Формы | |
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.56 | g/cm³ | ASTM D297 |
Твердость | Номинальное значение | Единица измерения | Метод испытания |
---|
Твердость дюрометра (Shore A) | 70 | | ASTM D2240 |
Эластомеры | Номинальное значение | Единица измерения | Метод испытания |
---|
Tensile Stress (100% Strain) | 2.62 | MPa | ASTM D412 |
Прочность на растяжение (Break) | 19.8 | MPa | ASTM D412 |
Удлинение при растяжении (Break) | 340 | % | ASTM D412 |
Тепловой | Номинальное значение | Единица измерения | |
---|
Service Temperature | -7 to 232 | °C | |