Andur RT 9002 AP/Curene® 107
Описание материалов:
Andur RT 9002 AP is a low viscosity liquid prepolymer which can be processed and cured at room temperature with Curene 107 to yield an elastomer with a hardness of 88 to 92 Shore A. This system has a extended potlife of about 25 minutes that can be adjusted using oleic acid catalyst.
Andur RT 9002 AP is recommended where room temperature processing and curing is desired with minimal elastomer shrinkage.
Главная Информация | |
---|
Характеристики | |
Формы | |
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.21 | g/cm³ | ASTM D792 |
Твердость | Номинальное значение | Единица измерения | Метод испытания |
---|
Твердость дюрометра (Shore A) | 90 | | ASTM D2240 |
Эластомеры | Номинальное значение | Единица измерения | Метод испытания |
---|
Tensile Stress | | | ASTM D412 |
100% strain | 5.45 | MPa | ASTM D412 |
300% strain | 8.27 | MPa | ASTM D412 |
Прочность на растяжение (Yield) | 14.5 | MPa | ASTM D412 |
Удлинение при растяжении (Break) | 600 | % | ASTM D412 |
Сопротивляемость Bayshore | 48 | % | ASTM D2632 |
Термокомплект | Номинальное значение | Единица измерения | Метод испытания |
---|
Срок службы горшка | 25 | min | |
Терморегулирующая вязкость (25°C) | 690 | cP | ASTM D2393 |
Время демолд (22°C) | 6.0 | min | |
Дополнительная информация |
---|
Specific Gravity, ASTM D792, 68°F: 1.21 g/mlDurometer Hardness, ASTM D2240, Shore A: 88 to 92Die C Tear, ASTM D1004: 240 pliAverage Split Tear, ASTM D1938: 105 pliMixing Weight Ratio: 100 to 14.8Mixing Volume Ratio: 100 to 12.2Recommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 50°F: 2.8 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 55°F: 2.6 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 60°F: 2.4 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 65°F: 2.1 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 70°F: 1.9 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 75°F: 1.7 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 80°F: 1.5 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 85°F: 1.3 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 90°F: 1.1 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 95°F: 0.9 ccRecommended oleic acid catalyst volume required per 100 gm to achieve 8 min pot life at 100°F: 0.7 cc |