Описание материалов:
Andur 7500-DP is a polyether (PPG) based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 72 to 75 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.03 | g/cm³ | ASTM D792 |
Термокомплект | Номинальное значение | Единица измерения | Метод испытания |
---|
Терморегулирующая вязкость | | | ASTM D2393 |
70°C | 2000 | cP | ASTM D2393 |
100°C | 425 | cP | ASTM D2393 |
Дополнительная информация |
---|
NCO: 6.8 to 7.2%Specific Gravity, ASTM D792, 77°F: 1.03 g/mlSpecific Gravity, ASTM D792, 212°F: 0.995 g/ml |