Описание материалов:
Our new crosslinkable CompaMid® PA 6.6 compounds are thermoplastic polymers which behave like elastomers over a wide temperature range as a result of beta radiation cross-linking. Thanks to crosslinking, the originally thermoplastic material can withstand significantly higher temperatures of up to 400°C, thus providing greater shape retention under thermal load. Due to its excellent performance profile, crosslinkable CompaMid® PA 6.6 can replace costly high-performance plastics such as PPA, PPS or LCP in many cases. No mould changes are required when switching from standard PA 6.6 to CompaMid® PA 6.6, and the process parameters also remain the same.
Electrical Applications
Thanks to their outstanding electrical and mechanical properties, crosslinkable CompaMid ® PA 6.6 compounds are ideally suited for applications in the electrical and electronics industries.
Automotive Applications
Crosslinked components made of CompaMid ® PA 6.6 are used in the engine bay and exhaust system, where requirements are the toughest for heat resistance and shape retention, as well as resistance to salts, chemicals and corrosive media.
| Главная Информация | |
|---|
| Характеристики | - Crosslinkable
- Хорошие электрические свойства
|
| Физический | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Плотность | 1.35 | -- | g/cm³ | ISO 1183 |
| Формовочная усадка 1 | | | | ISO 294-4 |
| Across Flow
: 80°C | 1.0 | -- | % | |
| Flow
: 80°C | 0.95 | -- | % | |
| Поглощение воды | | | | ISO 62 |
| Saturation, 23°C | 6.0 | -- | % | |
| Equilibrium, 23°C, 50% RH | 1.5 | -- | % | |
| Номер вязкости | 140 | -- | cm³/g | ISO 307 |
| Механические | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Модуль растяжения | 4500 | 1800 | MPa | ISO 527-2/1 |
| Tensile Stress | | | | ISO 527-2/50 |
| Yield | 95.0 | -- | MPa | |
| Break | 85.0 | 45.0 | MPa | |
| Растяжимое напряжение | | | | ISO 527-2/50 |
| Yield | 7.5 | -- | % | |
| Break | 5.0 | > 50 | % | |
| Воздействие | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Ударная прочность | | | | ISO 179/1eA |
| -30°C | 2.0 | 2.0 | kJ/m² | |
| 23°C | 4.0 | 5.0 | kJ/m² | |
| Charpy Unnotched Impact Strength | | | | ISO 179/1eU |
| -30°C | 20 | 20 | kJ/m² | |
| 23°C | 30 | > 100 | kJ/m² | |
| Тепловой | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Heat Deflection Temperature | | | | |
| 0.45 MPa, Unannealed | 195 | -- | °C | ISO 75-2/B |
| 1.8 MPa, Unannealed | 225 | -- | °C | ISO 75-2/A |
| Температура плавления | 260 | -- | °C | ISO 11357-3 |
| Heat Distortion | < 400 | < 400 | °C | |
| Электрический | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Удельное сопротивление поверхности | 1.0E+10 | -- | ohms | IEC 60093 |
| Сопротивление громкости | 1.0E+15 | -- | ohms·cm | IEC 60093 |
| Относительная проницаемость (1 MHz) | 3.50 | -- | | IEC 60250 |
| Comparative Tracking Index (Solution A) | 550 | -- | V | IEC 60112 |
| Воспламеняемость | Сухой | Состояние | Единица измерения | Метод испытания |
|---|
| Огнестойкость (0.800 mm) | HB | -- | | UL 94 |
| Примечание |
|---|
| 1 . | 260 °CWZ, 600 Bar |