Описание материалов:
Vydyne R633H05 is 33% glass-fiber reinforced PA66/6 copolymer resin for superior surface appearance. Available in black, this injection-molding grade resin is lubricated for machine feed and mold release.
Vydyne R633H05 has tensile strength and modulus properties just below aluminum and zinc and can replace these metals in numerous applications due to an excellent balance of properties. Reduction in production costs, energy consumption, and part weight are key advantages of Vydyne glass-reinforced PA66/6 resins over aluminum and/or zinc die-cast parts.
Vydyne R633H05 is specially formulated to minimize the oxidative and thermal degradation of the PA66/6 copolymer when exposed to elevated temperatures for extended periods of time. Product provides improved retention of physical properties under exposure to longterm heat.
Vydyne R633H05 provides a higher heat distortion temperature, better resistance to creep, higher impact and better dimensional stability compared with unreinforced PA66/6. This product also provides a combination of excellent surface appearance with high tensile and modulus properties. This property balance enables usage of Vydyne R633H05 in applications where aesthetics and performance are important.
Typical Applications/End Uses:
Vydyne R633H05 resin has been used for many under-the-hood automotive applications, motor housings for power tools, and garden appliances. These resins have also been used in miscellaneous brackets, gears and clips that require high rigidity and strength.
Главная Информация | |
---|
Наполнитель/армирование | - Стекловолокно, 33% наполнитель по весу
|
Добавка | |
Характеристики | - Сополимер
- Хороший выпуск пресс-формы
- Хорошая поверхность
- Стабилизация тепла
- Высокая прочность на растяжение
- Смазка
|
Используется | - Автомобильная крышка под капот
- Шестерни
- Корпуса
- Оборудование для газонов и сада
- Замена металла
- Электропитание/другие инструменты
|
Рейтинг агентства | - Астм д 4066 PA112G35
- Астм д 6779 PA082G35
|
Номер файла UL | |
Внешний вид | |
Формы | |
Метод обработки | |
Физический | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Плотность | 1.39 | -- | g/cm³ | ISO 1183 |
Формовочная усадка | | | | ISO 294-4 |
Across Flow
: 23°C, 2.00 mm | 0.90 | -- | % | |
Flow
: 23°C, 2.00 mm | 0.40 | -- | % | |
Поглощение воды | | | | ISO 62 |
23°C, 24 hr | 1.3 | -- | % | |
Equilibrium, 23°C, 50% RH | 2.3 | -- | % | |
Механические | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Модуль растяжения (23°C) | 10800 | 8000 | MPa | ISO 527-2 |
Tensile Stress (Break, 23°C) | 184 | 130 | MPa | ISO 527-2 |
Растяжимое напряжение (Break, 23°C) | 4.0 | 6.0 | % | ISO 527-2 |
Флекторный модуль (23°C) | 8800 | 6800 | MPa | ISO 178 |
Flexural Strength (23°C) | 255 | 195 | MPa | ISO 178 |
Poisson's Ratio | 0.40 | -- | | ISO 527-2 |
Воздействие | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Ударная прочность | | | | ISO 179/1eA |
-30°C | 11 | 15 | kJ/m² | |
23°C | 12 | 25 | kJ/m² | |
Charpy Unnotched Impact Strength | | | | ISO 179/1eU |
-30°C | 44 | 91 | kJ/m² | |
23°C | 51 | 92 | kJ/m² | |
Зубчатый изод ударная прочность | | | | ISO 180 |
-30°C | 12 | 19 | kJ/m² | |
23°C | 13 | 22 | kJ/m² | |
Тепловой | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Heat Deflection Temperature | | | | |
0.45 MPa, Unannealed | 230 | -- | °C | ISO 75-2/B |
1.8 MPa, Unannealed | 220 | -- | °C | ISO 75-2/A |
Температура плавления | 233 | -- | °C | ISO 11357-3 |
CLTE | | | | ISO 11359-2 |
Flow
: 23 to 55°C, 2.00 mm | 1.5E-5 | -- | cm/cm/°C | |
Transverse
: 23 to 55°C, 2.00 mm | 1.0E-4 | -- | cm/cm/°C | |
Электрический | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Дуговое сопротивление (3.00 mm) | PLC 5 | -- | | ASTM D495 |
Comparative Tracking Index (3.00 mm) | 250 to 399 | -- | V | IEC 60112 |
Высокоусиленное дуговое зажигание (HAI) | | | | UL 746 |
0.750 mm | PLC 0 | -- | | |
1.50 mm | PLC 0 | -- | | |
3.00 mm | PLC 0 | -- | | |
Высоковольтная скорость отслеживания дуги (HVTR) | PLC 2 | -- | | UL 746 |
Зажигание горячей проволоки (HWI) | | | | UL 746 |
0.750 mm | PLC 4 | -- | | |
1.50 mm | PLC 4 | -- | | |
3.00 mm | PLC 3 | -- | | |
Воспламеняемость | Сухой | Состояние | Единица измерения | Метод испытания |
---|
Огнестойкость | | | | UL 94 |
0.750 mm | HB | -- | | |
1.50 mm | HB | -- | | |
3.00 mm | HB | -- | | |
Инъекция | Сухой | Единица измерения | |
---|
Температура сушки | 80.0 | °C | |
Время сушки | 4.0 | hr | |
Рекомендуемый Макс измельчения | 25 | % | |
Задняя температура | 280 to 310 | °C | |
Средняя температура | 280 to 310 | °C | |
Передняя температура | 280 to 310 | °C | |
Температура сопла | 280 to 310 | °C | |
Температура обработки (расплава) | 285 to 305 | °C | |
Температура формы | 65.0 to 95.0 | °C | |