Описание материалов:
Description:
E10101A is a cross-linked emulsion styrene-butadiene copolymer with divinyl benzene, using a mix of rosin and fatty acid as emulsifier. It is coagulated with Aluminum-acid and stabilized with a non-staining antioxidant. It is produced in acordance with good manufacturing practices and complies with FDA 21 CFR §175.300, §177.1210 and §178.3910 for use in food contact applications.
Applications:
E10101A gives excellent dimensional stability to compounds, reduces die swell and shrinkage in extruded products. It is also recommended for improving cohesive strength in adhesives and sealants which will be in contact with food or beverages.
Главная Информация | |
---|
Характеристики | - Антиоксидант
- Сополимер
- Приемлемый пищевой контакт
- Хорошая адгезия
- Хорошая стабильность размеров
- Устойчивый к пятнам
|
Используется | - Клеи
- Неспецифические пищевые приложения
|
Рейтинг агентства | - Управление по санитарному надзору за качеством пищевых продуктов и медикаментов 21 CFR 175,300
- Управление по санитарному надзору за качеством пищевых продуктов и медикаментов 21 CFR 177,1210
- Управление по санитарному надзору за качеством пищевых продуктов и медикаментов 21 CFR 178,3910
|
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Вязкость Mooney (ML 1+4, 100°C) | 115 | MU | ASTM D1646 |
Содержание золы | < 0.80 | % | ASTM D5667 |
Органическая кислота | 4.3 to 6.3 | % | ASTM D5774 |
Усадка | < 15 | % | ASTM D1917 |
Мыло | < 0.30 | % | ASTM D5774 |
Содержание стирола-
Скрепленный | 42 to 45 | % | ASTM D5775 |
Летучее вещество | < 0.80 | % | ASTM D5668 |
Механические | Номинальное значение | Единица измерения | Метод испытания |
---|
Модуль растяжения | 13.1 | MPa | ASTM D3185 |
Прочность на растяжение | 15.9 | MPa | ASTM D3185 |
Удлинение при растяжении (Break) | 360 | % | ASTM D3185 |