Описание материалов:
Royaltherm 1411A is a modified EPDM with a special silicone rubber.
Royaltherm 1411A is supplied as a base compound that can be vulcanized with peroxides or sulfur/accelerator systems. Royaltherm 1411A is 30 - 40 Durometer when vulcanized with 1.8 phr of dicumyl peroxide. It can be blended with Royaltherm 1721 for intermediate hardness applications.
Royaltherm 1411A is recommended for applications that require lower tensile strength than Royaltherm 1721. Royaltherm 1411A is also recommended for applications that require retention of mechanical strength at elevated temperatures, weather and moisture resistance, electrical stability and compression recovery at low temperatures.
Главная Информация | |
---|
Характеристики | - Хорошая устойчивость к погоде
- Высокая термостойкость
- Влагостойкий
- Вулканизируемый
|
Используется | |
Внешний вид | |
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 0.940 to 1.10 | g/cm³ | ASTM D792, ISO 1183 |
Вязкость Mooney (ML 1+4, 100°C) | 27 to 37 | MU | ASTM D1646 |
Твердость | Номинальное значение | Единица измерения | Метод испытания |
---|
Твердость дюрометра 1(Shore A) | 30 to 40 | | |
Эластомеры | Номинальное значение | Единица измерения | Метод испытания |
---|
Прочность на растяжение | > 7.00 | MPa | ASTM D412 |
Удлинение при растяжении (Break) | > 700 | % | ASTM D412 |
Примечание |
---|
1 . | Peroxide-cured |