Описание материалов:
Andur 82-DGP is a polyether (PTMG) based liquid, isocyanate terminated prepolymer. An elastomer with a hardness of 82 to 85 Shore D is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various polyols and their combinations with Curene 442 and other diamines, or by the use of plasticizers.
| Физический | Номинальное значение | Единица измерения | Метод испытания |
|---|
| Удельный вес | 1.14 | g/cm³ | ASTM D792 |
| Термокомплект | Номинальное значение | Единица измерения | Метод испытания |
|---|
| Терморегулирующая вязкость | | | ASTM D2393 |
| 70°C | 1700 | cP | ASTM D2393 |
| 100°C | 290 | cP | ASTM D2393 |
| Дополнительная информация |
|---|
| NCO: 10.8 to 11.2%Specific Gravity, ASTM D792, 77°F: 1.14 g/mlSpecific Gravity, ASTM D792, 212°F: 1.12 g/ml |