Описание материалов:
Andur 8 APLM is a polyester based liquid, toluene diisocyanate terminated prepolymer. An elastomer with a hardness of 79 to 82 Shore A is obtained when this prepolymer is cured with Curene 442 [4,4'-methylene-bis (orthochloroaniline)]. Elastomers of lower hardness can be obtained by reaction with various poyols and their combination with Curene 442 and other diamines, or through the use of plasticizers.
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Удельный вес | 1.16 | g/cm³ | ASTM D792 |
Термокомплект | Номинальное значение | Единица измерения | Метод испытания |
---|
Терморегулирующая вязкость | | | ASTM D2393 |
70°C | 3700 | cP | ASTM D2393 |
100°C | 1030 | cP | ASTM D2393 |
Дополнительная информация |
---|
NCO: 3 to 3.45%Specific Gravity, ASTM D792, 70°F: 1.16 g/mlSpecific Gravity, ASTM D792, 212°F: 1.14 g/ml |
Тип материала |
Категория |
Производитель |
Vytaflex® 50 |
PUR, Unspecified |
Smooth-On, Inc
|
Xuchuan XCA-4525A |
PUR, Unspecified |
Xuchuan Chemical (Suzhou) Co., Ltd
|
Evermore PUR SS-1058NHR |
PUR, Unspecified |
Evermore Chemical Industry Co., Ltd.
|
Huafon JF-D-C5902 |
PUR, Unspecified |
Huafon Group Co., Ltd.
|
Huafon JF-P-550S / JF-I-650 |
PUR-Ether |
Huafon Group Co., Ltd.
|
HydroThane™ 93A |
PUR, Unspecified |
CardioTech International, Inc.
|