Monprene CP-38225 XRD2 is a high performance thermoplastic elastomer designed for a variety of consumer product applications requiring a soft, rubber-like feel. Monprene CP-38225 XRD2 is a low hardness, low density, clear grade that is suitable for both injection molding and extrusion.
Главная Информация
Характеристики
  • Низкий удельный вес
  • Без наполнителей
  • Низкая плотность
  • Гладкость
  • Обрабатываемость, хорошая
  • Хорошая адгезия
  • Средняя степень жидкости
  • Хорошая химическая стойкость
  • Смазка
  • Твердость, низкая
Используется
  • Ручка
  • Шайба
  • Спортивные товары
  • Канцелярские принадлежности
  • Замена резины
  • Применение потребительских товаров
  • Ручка
Соответствие RoHS
  • Соответствие RoHS
Внешний вид
  • Прозрачный/прозрачный
Формы
  • Частицы
Метод обработки
  • Экструзия
  • Литье под давлением
ФизическийНоминальное значениеЕдиница измеренияМетод испытания
Удельный вес 0.878g/cm³ASTM D792
Массовый расход расплава (MFR) (190°C/2.16 kg)13g/10 minASTM D1238
ТвердостьНоминальное значениеЕдиница измеренияМетод испытания
Твердость дюрометра ASTM D2240
    Shore A, 1 second, injection molding 28ASTM D2240
    Shore A, 5 seconds, injection molding 25ASTM D2240
ЭластомерыНоминальное значениеЕдиница измеренияМетод испытания
Tensile Stress 1ASTM D412
    Transverse flow : 100% strain 0.600MPaASTM D412
    Flow : 100% strain 0.731MPaASTM D412
    Transverse flow : 300% strain 1.34MPaASTM D412
    Flow : 300% strain 1.81MPaASTM D412
Прочность на растяжение 2ASTM D412
    Transverse flow : Fracture 7.05MPaASTM D412
    Flow : Fracture 6.90MPaASTM D412
Удлинение при растяжении 3ASTM D412
    Transverse flow : Fracture 560%ASTM D412
    Flow : Fracture 520%ASTM D412
Tear Strength 4ASTM D624
    Transverse flow 23.3kN/mASTM D624
    Flow 21.2kN/mASTM D624
Комплект сжатия 5(23°C, 22 hr)19%ASTM D395B
Юридическое заявление
The information and recommendations contained in this bulletin are, to the best of our knowledge, accurate and reliable but no guarantee of their accuracy is made. All products are sold upon condition that purchasers shall make their own tests to determine the suitability of such products for their particular purposes and uses and purchaser assumes all risks and liability for the results of use of the products, including use in accordance with seller's recommendations. Nothing in this bulletin constitutes permission or a recommendation to practice or use any invention covered by any patent owned by this company or others. There is no warranty of merchantability and there are no other warranties for the products described. For detailed Product Stewardship information, please contact us. Any product of Teknor Apex, including product names, shall not be used or tested in medical or food contact applications without the prior written acknowledgement of Teknor Apex as to the intended use. Please note that some products may not be available in one or more countries.
ИнъекцияНоминальное значениеЕдиница измерения
Задняя температура 171 - 204°C
Средняя температура 171 - 204°C
Передняя температура 171 - 204°C
Температура сопла 171 - 204°C
Температура обработки (расплава) 171 - 204°C
Температура формы 16 - 32°C
Давление впрыска 1.38 - 5.52MPa
Скорость впрыска Fast
Back Pressure 0.172 - 0.689MPa
Screw Speed 50 - 100rpm
Подушка 3.81 - 25.4mm
Инструкции по впрыску
Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to 4 hours at 150°F (65°C).
ЭкструзияНоминальное значениеЕдиница измерения
Зона цилиндра 1 темп. 160 - 193°C
Зона цилиндра 2 температура. 160 - 193°C
Зона цилиндра 3 темп. 160 - 193°C
Зона цилиндра 4 темп. 160 - 193°C
Зона цилиндра 5 темп. 160 - 193°C
Температура матрицы 160 - 193°C
Инструкции по экструзии
Screw Speed: 30 to 100 rpm
Примечание
1 .C mold, 510mm/min
2 .C mold, 510mm/min
3 .C mold, 510mm/min
4 .C mold, 510mm/min
5 .Type 1
Тип материала Категория Производитель
Telcar® TL-2590F TPE Teknor Apex Company
THERMOLAST® K TC7GPN (Series: GP/FG) TPE KRAIBURG TPE
Dryflex® 4103 TPE ELASTO
Gallonprene® GP520-7002 TPE Shenzhen Sungallon Rubber & Plastic Corporation Limited
Franprene TGA 2270 TPE Franplast S.r.l.
Elastocon® CLR40 TPE Elastocon TPE Technologies
Получите информацию об этом продукте следующим способом.
Телефон+086 13424755533
EMAIL US sales@su-jiao.com

Служба поддержки клиентов Вичат

Copyright © russianpolymer.com All Rights Reserved
Получите информацию об этом продукте следующим способом.

Служба поддержки клиентов Вичат
Свяжитесь с нами