Описание материалов:
438 is a hexene copolymer linear low density polyethylene, designed for a variety of general purpose applications. 438 is formulated with process aid and a stabilisation package but contains no slip of antiblock additives.
438 is intended for general purpose blending applications such as film for liners. 438 is not recommended for use in outdoor applications (especially applications where there may be prolonged exposure to sunlight, eg. agricultural films) without the addition of appropriate Hindered Amine based Light Stabilisers (HALS).
438 is suitable for food contact applications and conforms to the requirements of the United States Food and Drug Administration CFR 21 177.1520, paragraph (c), item 3.1.
Главная Информация | |
---|
Добавка | - Стабилизатор обработки
- Вспомогательные средства для обработки
|
Характеристики | - Высокая гладкость
- Сополимер
- Устойчивость к царапинам
- Соответствие пищевого контакта
|
Используется | |
Рейтинг агентства | - FDA 21 CFR 177,1520 (c) 3,1
|
Формы | |
Метод обработки | |
Физический | Номинальное значение | Единица измерения | Метод испытания |
---|
Плотность | 0.922 | g/cm³ | ASTM D1505 |
Массовый расход расплава (MFR) (190°C/2.16 kg) | 0.80 | g/10 min | ASTM D1238 |
Механические | Номинальное значение | Единица измерения | Метод испытания |
---|
Коэффициент трения (Blown Film) | 0.50
0.50 | | ASTM D1894 |
Пленки | Номинальное значение | Единица измерения | Метод испытания |
---|
Толщина пленки протестирована | 25
50 | µm | |
Сектантный модуль | | | ASTM D882 |
2% secant, MD
: 25 µm | 190 | MPa | ASTM D882 |
2% secant, MD
: 50 µm | 200 | MPa | ASTM D882 |
2% secant, TD
: 25 µm | 200 | MPa | ASTM D882 |
2% secant, TD
: 50 µm | 230 | MPa | ASTM D882 |
Прочность на растяжение | | | ASTM D882 |
MD
: Yield, 25 µm | 9.00 | MPa | ASTM D882 |
MD
: Yield, 50 µm | 10.0 | MPa | ASTM D882 |
TD
: Yield, 25 µm | 11.0 | MPa | ASTM D882 |
TD
: Yield, 50 µm | 12.0 | MPa | ASTM D882 |
MD
: Break, 25 µm | 47.0 | MPa | ASTM D882 |
MD
: Break, 50 µm | 46.0 | MPa | ASTM D882 |
TD
: Break, 25 µm | 41.0 | MPa | ASTM D882 |
TD
: Break, 50 µm | 42.0 | MPa | ASTM D882 |
Удлинение при растяжении | | | ASTM D882 |
MD
: Break, 25 µm | 900 | % | ASTM D882 |
MD
: Break, 50 µm | 1100 | % | ASTM D882 |
TD
: Break, 25 µm | 1000 | % | ASTM D882 |
TD
: Break, 50 µm | 1100 | % | ASTM D882 |
Ударное падение Dart | | | ASTM D1709 |
25 µm, blown film | 160 | g | ASTM D1709 |
50 µm, blown film | 260 | g | ASTM D1709 |
Elmendorf Tear Strength | | | ASTM D1922 |
MD
: 25 µm | 290 | g | ASTM D1922 |
MD
: 50 µm | 670 | g | ASTM D1922 |
TD
: 25 µm | 510 | g | ASTM D1922 |
TD
: 50 µm | 1100 | g | ASTM D1922 |
Оптический | Номинальное значение | Единица измерения | Метод испытания |
---|
Блеск | | | ASTM D2457 |
25.0 µm, blown film | 64 | | ASTM D2457 |
50.0 µm, blown film | 67 | | ASTM D2457 |
Haze | | | ASTM D1003 |
25.0 µm, blown film | 8.0 | % | ASTM D1003 |
50.0 µm, blown film | 10 | % | ASTM D1003 |
Дополнительная информация |
---|
Film properties taken from blown film processed at a blow up ratio of 3.5:1. |